Creep Tester No.145-SV | YASUDA SEIKI

creep testing measures the deformation of materials (creep and stress relaxation) under a constant load, at specific temperatures, and long time. The system utilizes a servomotor control combined with a load cell, which helps minimize impact forces when a specimen fractures. It is capable of performing tests with a maximum capacity of 5–10 kN.

Key Feature

  • Stress Relaxation Measure the reduction in stress long time in a material when held at a constant elongation.
  • Long-term Creep measure and analyze deformation from Creep deflection under tension, compression, and bending for the purpose of predicting service life.
  • Measure deformation at a high precision0.01 mm magnetostrictive transducer is employed to continuously and consistently record the expansion or contraction of the workpiece.
  • Supports testing of 3, 6, and up to 10 specimens: Available in versions featuring pulley, balance scale, or servomotor systems.

Reference Standards

JIS K7115、ASTM D2990、ISO 899-1

Specification

Specification Details
Number of Test Samples 3, 6, or 10 samples per test
Test Sample Refer to JIS K7161, JIS K6263
Loading System Servomotor
Load Max. 5 kN (500 kgf), Max. 10 kN (1,000 kgf)
Load Measurement Load Cell
Displacement Measurement Magnetostrictive linear displacement transducer (resolution: 0.01 mm, measurement range: 100 mm)
Temperature Max. 200°C (Option: 300°C)
PC Software Available for Windows
Options Compression frame and platens, bend fixtures, low-temperature chamber,
temperature and humidity chamber, split chamber, displacement measurement
within the gauge length, stress relaxation test specification
Power Source Vary according to the tester specs.
Dimensions and Weight (Approx.) Vary according to the tester specs.

FAQ Section

Q: How does the Creep Tester (Model No. 145) differ from a standard tensile test?

A: A typical tensile test involves pulling a sample at a constant speed until it breaks to determine its maximum strength. However, Creep Tester the application of compressive or tensile force. Maintained in a fixed state for a long time. (e.g., over several hours or days) to observe the stretching or deformation of a material as time and temperature change—a process essential for estimating its actual service life.

Q: Which model—No.145-A, No.145-B, or No.145-SV—is most suitable for the task?

A: For testing specimens under low compressive force (up to 500 N), we recommend the following model: No.145-A (Pulley) For plastic or rubber that require a higher pressing force of up to 5 kN, we recommend the following model: No.145-B (Balance) However, if you require a system that saves space, reduces the impact force when a specimen breaks, and supports testing Stress Relaxation Model selection guide No.145-SV (Servomotor)

Q: Can the device perform tests under high-temperature conditions?

A: Yes Test chamber capable of heating under standard conditions up to a maximum . 200°C And optional features can be selected to extend the temperature range up to 300°C it can be integrated with an environmental chamber (temperature and humidity control cabinet) to simulate the most realistic environmental conditions.